What it is

Kind
Frits
Formula
SiO₂ 49.6%, B₂O₃ 18%, MgO 0.1%, Al₂O₃ 7.5%, Na₂O 8.8%, K₂O 1.7%, CaO 14.1%
Also called
Borax (E) Frit, Borax E Frit, Waterground & Dried Borax E Frit, Potterycrafts P2953
Sold in
UK
Similar materials
Standard Borax Frit (Potclays 2263)
Source
Potterycrafts 'Waterground & Dried Borax E Frit' product page

Potterycrafts' standard borax frit, a general-purpose leadless frit for earthenware glazes. Expansion 8.3 x 10^-6/°C, firing range 900-1100 °C.

Oxide analysis and unity formula

Glazecalc has the analysis of Borax Frit (Potterycrafts P2953) as weight percent of the raw material. The unity contribution is the moles of each oxide in the amount of Borax Frit (Potterycrafts P2953) that holds 1.0 mole of flux, which is how Glazecalc adds it into a recipe's unity formula.

Oxides in Borax Frit (Potterycrafts P2953)
Oxide Weight % Unity contribution
SiO₂49.61.994
B₂O₃180.625
MgO0.10.006
Al₂O₃7.50.178
Na₂O8.80.343
K₂O1.70.044
CaO14.10.607
Equivalent weight
241.57
Fired weight
241.57
Loss on ignition
0%

The equivalent weight is the grams of Borax Frit (Potterycrafts P2953) that hold 1.0 mole of flux. The fired weight is what is left of that after firing.

Hazards and safety

Hazards: Not classified (Potterycrafts SDS P2953; under 1% quartz); breathing the dust over long periods raises the risk of lung disease.

Glazecalc shows the hazard wording as its record gives it. It is not a full risk assessment, so read the safety data sheet from your supplier. Before you handle any glaze material, read Safe mixing and ventilation and Glaze safety at home.