What it is

Kind
Fluxes
Formula
Ca₃(PO₄)₂
Source
Theoretical formula

Tricalcium phosphate. Real bone ash may contain a little CaCO₃ and so a small LOI.

Oxide analysis and unity formula

Glazecalc has the analysis of Bone Ash as moles of each fired oxide per formula. The unity contribution is the moles of each oxide in the amount of Bone Ash that holds 1.0 mole of flux, which is how Glazecalc adds it into a recipe's unity formula.

Oxides in Bone Ash
Oxide Moles Unity contribution
CaO31.000
P₂O₅10.333
Equivalent weight
103.39
Fired weight
103.39
Loss on ignition
0%

The equivalent weight is the grams of Bone Ash that hold 1.0 mole of flux. The fired weight is what is left of that after firing.

Hazards and safety

Hazards: Warning (Potterycrafts SDS): H302 harmful if swallowed; H315 causes skin irritation; H319 causes serious eye irritation; H335 dry dust may cause respiratory irritation.

Glazecalc shows the hazard wording as its record gives it. It is not a full risk assessment, so read the safety data sheet from your supplier. Before you handle any glaze material, read Safe mixing and ventilation and Glaze safety at home.